7075 Aluminum: Properties, Uses, and Where to Order
MetalNow · October 29, 2026
What's in 7075 aluminum
7075 belongs to the 7000 series, where zinc is the main alloying element. Magnesium and copper are added for extra strength. Here are the standard composition limits:
Zinc: 5.1–6.1%
Magnesium: 2.1–2.9%
Copper: 1.2–2.0%
Chromium: 0.18–0.28%
Iron: 0.50% max
Silicon: 0.40% max
Manganese: 0.30% max
Titanium: 0.20% max
Aluminum: balance
The zinc and magnesium do the heavy lifting. During heat treatment they form tiny particles that strengthen the metal from within. The copper adds strength too, but it's also part of why 7075 is less corrosion resistant than 6061, which uses magnesium and silicon instead.
7075 aluminum properties
These are typical values for 7075-T6 and T651, the tempers you'll usually find in stock:
Tensile strength: about 83 ksi (572 MPa)
Yield strength: about 73 ksi (503 MPa)
Elongation: about 11% (lower in thick plate)
Hardness: about 150 Brinell
Modulus of elasticity: 10,400 ksi (71.7 GPa)
Density: 0.102 lb/in³ (2.81 g/cm³)
Thermal conductivity: roughly 130 W/m·K
How that compares: 6061-T6 typically has about 45 ksi tensile and 40 ksi yield. So 7075-T6 is nearly twice as strong at almost the same weight.
One thing that doesn't change is stiffness. 7075 and 6061 have about the same modulus, so a 7075 part flexes about as much as the same 6061 part under the same load. 7075 can take far more load before it bends permanently or breaks, but it won't make a flimsy design stiffer. If deflection is the problem, change the geometry, not the alloy.
Common 7075 tempers
The letters and numbers after "7075" describe how the metal was heat treated. That changes its strength and behavior a lot.
7075-O (annealed): soft and formable, at less than half the strength of T6. It's used when a part will be formed first and heat treated afterward.
7075-T6: solution heat treated and artificially aged to peak strength. This is the most common temper for bar and rod.
7075-T651: T6 that's also stress-relieved by stretching. This is the standard for plate, because the stress relief keeps it from warping when you machine away a lot of material.
7075-T73 / T7351: "overaged" past peak strength. You give up some strength (roughly 10–15%) for much better resistance to stress corrosion cracking. It's used for aerospace parts under constant load, like landing gear and wing fittings.
For most machining jobs, T6 bar or T651 plate is what you want. Choose T73 when the part will be under sustained stress in a damp or corrosive environment.
What 7075 does well, and where it falls short
Where it shines
Strength-to-weight: few aluminum alloys come close. It's often used in place of steel where weight matters.
Machinability: in T6 and T651 it machines cleanly, holds tight tolerances and gives a good surface finish. It's harder than 6061, so it produces smaller chips and less built-up edge.
Fatigue strength: it holds up well under repeated loading, which is why it's common in aircraft structures and performance parts.
Anodizing: it anodizes well for wear resistance and corrosion protection. Clear anodize can look a little more yellow or gray than on 6061.
Where it falls short
Welding: 7075 isn't considered weldable with standard arc processes like TIG and MIG. The weld area tends to crack, and it can fail later in service from stress corrosion. If a part has to be welded, use 6061, or a weldable 7000-series alloy like 7005. Friction stir welding is the exception, but it's specialized.
Corrosion resistance: it's lower than 6061 because of the copper content. It's also prone to stress corrosion cracking in the T6 temper. For outdoor or marine use, anodize or coat it, or choose T73.
Forming: in T6 it's hard and doesn't bend well. Tight bends will crack.
Cost: it typically costs more than 6061, so use it where you actually need the strength.
Common uses for 7075 aluminum
You'll find 7075 anywhere a part has to be strong without being heavy:
Aerospace: wing and fuselage structures, fittings and brackets. It's been an aircraft alloy since the 1940s.
Defense and firearms: rifle receivers, especially AR-15 upper and lower receivers, along with mounts and other high-stress components.
Automotive and motorsports: suspension parts, brackets and other performance components where saving weight matters.
Cycling and outdoor gear: bike components like chainrings and derailleur parts, and climbing gear like carabiners.
Tooling and molds: plastic injection molds and fixtures that need to be hard, stable and quick to machine.
Robotics and machinery: high-load arms, gears and shafts, where 6061 would bend or wear too quickly.
They all have the same need: high strength, low weight, and a machined part rather than a welded one.
7075 vs 6061: which do you need?
Most aluminum parts are made from 6061, and that's usually the right call. Here's how to decide.
Choose 7075 when:
The part carries high loads, and 6061 would yield or wear out.
Saving weight is important, and you need maximum strength in a small cross-section.
The part is machined, not welded.
You need a hard, stable material for molds, fixtures or precision parts.
Choose 6061 when:
The part will be welded.
It's going outdoors or near water, and you want better corrosion resistance without coating.
It needs to be bent or formed.
The strength of 6061 is enough, and you'd rather keep costs down.
Not sure? Start with 6061 and move to 7075 only if testing or calculations show you need it. For more on aluminum grades, see our guide to 6061 vs 6063 aluminum.
Where to order 7075 aluminum
MetalNow stocks 7075 aluminum in [bar, plate and other forms — confirm forms and tempers]. You can see your price online instantly, order as little as one piece, and get it cut to your exact size and shipped anywhere in the contiguous U.S. There's no quote to wait on and no minimum order, so it works just as well for a single prototype part as for a production run.
Not sure whether 7075 or 6061 is right for your part? Reach out to our team. With 25 years in metal distribution, we're glad to help you choose.
Related reading